Compositio chemica
Gradus | C≤ | Si≤ | Mn≤ | P≤ | S≤ | Ni | Cr |
201 | 0.15 | 1 | 5.50-7.50 | 0.5 | 0.03 | 3.50-5.50 | 16.00-18.00 |
202 | 0.15 | 1 | 7.50-10.00 | 0.5 | 0.03 | 4.00-6.00 | 17.00-19.00 |
304 | 0.08 | 1 | 2 | 0.041 | 0.03 | 8.00-11.00 | 18.00-20.00 |
304L | 0.03 | 1 | 2 | 0.041 | 0.03 | 8.00-12.00 | 18.00-20.00 |
309 | 0.2 | 1 | 2 | 0.04 | 0.03 | 12.00-1500 | 22.00-24.00 |
309S | 0.08 | 1 | 2 | 0.041 | 0.03 | 12.00-1500 | 22.00-24.00 |
310 | 0.25 | 1 | 2 | 0.04 | 0.03 | 19.00-22.00 | 24.00-26.00 |
310S | 0.08 | 1 | 2 | 0.041 | 0.03 | 19.00-22.00 | 24.00-26.00 |
316 | 0.08 | 1 | 2 | 0.041 | 0.03 | 10.00-14.00 | 16.00-18.00 |
316L | 0.03 | 1 | 2 | 0.041 | 0.03 | 10.00-14.00 | 16.00-18.00 |
316Ti | 0.08 | 1 | 2 | 0.041 | 0.03 | 10.00-14.00 | 16.00-18.00 |
410 | 0.15 | 1 | 1 | 0.04 | 0.03 | 0.6 | 11.50-13.50 |
430 | 0.12 | 0.12 | 1 | 0.04 | 0.03 | 0.6 | 16.00-18.00 |
Superficiem perfice Diver Coil
Superficiem Conclusio | Definition | Applicationem |
No.1 | Superficies per curationem caloris confecta et servantur vel processibus ibi respondentibus post volubilem calidum. | Eget lacus, pipe |
2B | Quibus confectis, post volvendum frigus, per curationem caloris, salsura vel alia aequivalentia curatio, postremo ex frigore volventia, quae opportuna nitorem dederunt. | Instrumentum medicinae, Cibus industriam, Materia constructio, vasa coquinaria. |
No.4 | Qui perfecti sunt expolitio cum No.150 ad No.180 abrasives de quibus in JIS R6001. | Culina, Vasa Electric, Aedificium constructione. |
Hairline | Qui perfecti poliuntur ita ut stricturas continuas expoliant utendo laesura congrui grani magnitudine. | Building Construction. |
BA/8K Speculum | Curatio illae processit cum calore claro post frigus volubilem. | Culina utensilia, instrumenta electrici, Aedificium const |
Cognitio Steel
●304
304 chalybs immaculata est materia valde versatilis, vulgo in armorum fabricatione et partium fabricandis, quae praestantiores altiore proprietates requirunt, inclusa repugnantia et formabilitas corrosionis.Ut resistentia inhaerens corrosio, chalybs immaculata saltem 18% chromium et 8% nickel continere debet.
Vexillum of
Compositio 304 ferri partes vitalis agit in eius corrosione resistentia et valore determinando.Etsi nickel (Ni) et chromium (Cr) praecipua elementa sunt, alia quoque membra involvi possunt.Productum vexillum specifica requisita pro 304 ferro specificat.Communiter intellegitur in industria quod si Ni contentum 8% excedit et Cr contentum 18% excedit, in 304 ferro collocari potest.Quam ob rem saepius 18/8 immaculatam ferrum dicitur.Notandum est, quod in signis ferris producti manifesti sunt regulae, et hae ordinationes variari possunt secundum formam et formam chalybi immaculati.